Ultraviolet (UV) radiation is one of the major risk factors of cataract (loss of eye-lens transparency). The influence of UVB radiation (300 nm, 100 mu W cm(-2)) on the activity and apparent kinetic constants (K-m and V-max) of rat lens hexokinase (HK;EC2.7.1.1), phosphofructokinase (PFK;EC2.7.1.11), isocitrate dehydrogenase (ICDH;EC1.1.1.41) and malate dehydrogenase (MDH;EC1.1.1.37) of energy metabolism has been investigated by irradiating the lens homogenate of three-and 12-month-old rats. In the three-month-old group specific activities of HK and PFK are reduced by 56 and 43 %, respectively, and there is no change in ICDH and MDH activities after a 24 h exposure. On the other hand, in the 12-month-old group the decreases are 72, 71, 24 and 16 % for HK, PFK. ICDH and MDH, respectively. UVB irradiation increases the apparent K-m of HK and PFK (in both age groups), whereas the K-m of ICDH and MDH is not altered. While the decrease in V-max of these enzymes due to UVB exposure is only marginal in three-month-old rats, it is more pronounced (significant) in 12-month-old rats. A similar decrease in enzyme activities of HK and PFK is also observe upon UVB exposure of the intact rat lens. The photoinduced changes in energy metabolism may in turn have a bearing on lens transparency, particularly at an older age.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Multistress aging of outdoor composite polymeric insulators continues to be a topic of interest for power transmission research community. Aging due to dry conditions alone at elevated temperatures and electric stress in the presence of UV radiation environment probably has not been explored. This paper deals with long-term accelerated multistress aging under the above conditions on full-scale 11 kV distribution class composite silicone rubber insulators. To evaluate the long-term synergistic effect of electric stress, temperature and UV radiation on insulators, they were subjected to accelerated aging in a specially designed multistress-aging chamber for 12000 hours. Chemical, physical and electrical changes due to degradation have been assessed using various techniques. It has been found that the content of low molecular weight molecules and hydrophobicity reduced significantly. Also, due to oxidation and aging there is appreciable increase in surface roughness and weight percentage of oxygen. Study is under progress and only intermediate results are presented in this paper.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

During the thermal decomposition of orthorhombic ammonium perchlorate (AP) at 230°C, where the decomposition is only up to 30 wt %, there is an accumulation in the solid of acids, the concentration of which increases up to 15% decomposition, after which it decreases till it reaches the original value. Similar observations have been made in the polystyrene (PS)/AP propellant systems. Aging studies of PS/AP propellants have been carried out earlier [1], where it has been shown that for the aged propellants the thermal decomposition (TD) rate at 230°C and 260°C and ambient pressure burning rate (Image ) both increase and this increase is due to the formation of reactive intermediate “polystyrene peroxide (PSP).” In the present studies it has been observed that during the aging of the propellant at 150°C, the acid is formed and gets accumulated in the propellant, which may also be responsible for the increase in TD rate and perhaps may be more effective than PSP.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The β-phase aging response of Cu–Al–Ni single crystal shape memory alloys (SMAs) within the temperature range of 473–573 K has been investigated. Alloys in austenitic (Cu–14.1Al–4Ni wt.%, alloy A) and martensitic (Cu–13.4Al–4Ni wt.%, alloy M) conditions at room temperature were considered. Aged samples show presence of β1′ and γ1′ martensites in both the alloys and formation of γ2 precipitates in the alloy A. The differential scanning calorimetry (DSC) thermograms of the aged samples show increase in transformation temperatures as well as transformation hysteresis with aging. Dynamic mechanical analysis (DMA) was conducted on both the alloys to ascertain the role of precipitates and martensitic transition on tan δ, which characterizes the damping behaviour of the material. With aging, a steady decrease in tan δ value was observed in both the alloys, which was attributed to the decrease in the number of interfaces per unit area with increasing aging temperature. Moreover, in alloy A, as the volume fraction of precipitate increases with aging, the movement of martensitic interfaces is restricted causing a decreased tan δ.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polymeric outdoor insulators are being increasingly used for electrical power transmission and distribution in the recent years. One of the current topics of interest for the power transmission community is the aging of such outdoor polymeric insulators. A few research groups are carrying out aging studies at room temperature with wet period as an integral part of multistress aging cycle as specified by IEC standards. However, aging effect due to dry conditions alone at elevated temperatures and electric stress in the presence of radiation environment has probably not been explored. It is interesting to study and understand the insulator performance under dry conditions where wet periods are either rare or absent and to estimate the extent of aging caused by multiple stresses. This paper deals with the long-term accelerated multistress aging on full-scale 11 kV distribution class composite silicone rubber insulators. In order to assess the long-term synergistic effect of electric stress, temperature and UV radiation on insulators, they are subjected to accelerated aging in a specially designed multistress-aging chamber for 3800 hours. All the stresses are applied at an accelerated level. Using a data acquisition system developed for the work, leakage current has been monitored in LabVIEW environment. Chemical changes due to degradations have been studied using Energy Dispersive X-Ray analysis, Scanning Electron Microscope and Fourier transform Infrared Spectroscopy. Periodically different parameters like low molecular weight (LMW) molecular content, hydrophobicity, leakage current and surface morphology were monitored. The aging study is under progress and only intermediate results are presented in this paper.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Terahertz time-domain spectroscopy has been carried out on a metallic film of polypyrrole (PPy doped by PF6). The sample was exposed to air to investigate how the conductivity of the film varies as a function of time. The absorption and dispersion of the film decrease during initial days, and then tend to saturate. The conductivity of unaged sample follows the Drude model, and upon aging the data fit to the localization-modified Drude model. The fitting parameters show that the number of charge carriers decreases during the aging process. The initial rapid decrease in conductivity suggests that some of the delocalized carriers are localized due to aging. (C) 2007 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The humid aging of composite propellants containing a terpolymer of polybutadiene, acrylic acid, and acrylonitrile (PBAN) as a binder has been studied as a function of aging temperature, relative humidity, and aging time. Three composite types - AP-PBAN, AP-Al-PBAN, and AP-(Al-Mg) alloy- PBAN - have been studied. The burning rates of all three propellant types were unaffected by aging. The calorimetric values of composites containing aluminum-magnesium alloy decreased on aging, and the lattice parameter of the alloy decreased to a value close to that of aluminum. Water absorption in all of the samples increased with increases in the temperature, relative humidity, and aging time. The compression strength of the nonmetalized and aluminized samples decreased on aging, whereas that of the composites containing the alloy increased. The latter effect has been traced to reaction of residual carboxyl groups on the polymer chains with magnesium, leading to cross-linking. The reaction between the -COOH groups and magnesium has been proved using infrared spectroscopy. (Author)

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In EHV and UHV power transmission lines, corona could occur even on well designed transmission line hardware and insulators especially under wet conditions. Corona if allowed to occur continuously can significantly damage the polymeric insulators used in such lines in the long run. This paper presents the experimental results of corona aging studies conducted on unfilled silicone rubber as well as filled silicone rubber nanocomposites. Corona aging studies were conducted on silicone rubber samples with filler concentrations of 0, 1, 2 and 3 % by wt of nanosilica for 25 h and 50 h. Needle-plane electrode geometry has been used to create the corona on the samples. Different characterization techniques such as Scanning Electron Microscopy, Energy Dispersive X-ray analysis, Hydrophobicity, Fourier Transform Infrared Spectroscopy, and Optical Profilometry have been used to assess the relative performance of the samples with respect to corona aging. Results indicate that at 3 wt %, the performance of the nanocomposite is much better than the unfilled silicon rubber which can be attributed to the modifications in the material caused by the size factor of the filler.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Al-7Si-0.3Mg is a commonly used commercial casting alloy because of its excellent castability combined with good mechanical properties. The post-casting heat treatment is one factor that affects the mechanical properties; during heat treat ment, a delay between solutionizing and artificial aging (delayed aging) leads to a reduction in hardness, ultimate tensile strength, and yield strength in the alloy. The investigation reported here was aimed at understanding the extent to which the harmful effect of delayed aging on hardness/strength can be nullified. The results obtained were explained using Pashley's kinetic model.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present study, 6061 Al metallic matrix was reinforced by 12.2 wt% df SiC particulates using liquid metallurgy route. The composite material thus obtained was extruded and characterized in the as-solutionized and peak aged conditions in order to delineate the effect of aging associated precipitation of secondary phases on the tensile fracture behavior of the composite samples. The results' of microstructural characterization studies carried out using scanning electron microscope revealed the increased presence of precipitated secondary phases in the metallic matrix and a more pronounced interfacial segregation of alloying elements in case of peak aged samples when compared to the as-solutionized samples. The results of the fractographic studies conducted on the as-solutionized samples revealed that the failure was dominated by the SiC particulates cracking while for the peak aged samples the fracture surface revealed a comparatively more pronounced SiC/6061 Al debonding and reduced SiC particulates cracking. This change in the failure behavior was rationalized in terms of embrittlement of the interfacial region brought about by the aging heat treatment and is correlated, in addition, with the mechanical properties of the composite samples in as-solutionized and peak aged conditions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Effect of aging on swelling and swell-shrink behavior of a compacted expansive soil is investigated in this paper. An expansive soil having a liquid limit of 100% is used for this purpose. Compacted specimens were prepared and aged for a predetermined number of days (7, 15, 30, and 90 days) to study their swelling and swell-shrink behavior. It has been shown that aging improves the resistance to compression of compacted specimens. The swelling potentials of specimens also decreased with aging. The dominant factors that influence the aging effects are the water content and degree of saturation at the beginning of the aging process. The changed behavior of aged specimens is attributed to particle rearrangements and formation of bonds, which affect the surface area absorbing water during swelling. The cyclic swell-shrink tests on aged specimens indicated that the differences in vertical displacement during the first swelling were eliminated in the subsequent cycles when specimens were shrunk more, but the aging effect was found to persist with cycles for specimens subjected to lower shrinkage magnitudes.